Evaluation of the Effect of Different Surface Treatments on the Bond Strength of Zirconia to Resin Cement
Main Article Content
Abstract
Background Zirconia, which is resistant to both chemical and acid attack, requires a surface modification to reliably bond with resin cement in the luting process. Various protocols (air-abrasion, silica-coating, etching, lasers, plasma, 10-MDP primer, and combinations thereof) have been suggested to improve adhesion of zirconia to resin cements, but no consensus has been reached based on hundreds of small in-vitro studies.
Objective To analyze the evidence published between 2020 and 2025 in order to evaluate the effect of various surface treatments on the adhesion strength of zirconia to resin cement.
Methods: A search for in vitro studies and secondary research on surface treatment of zirconia and the bond strength to resin-cement was performed in Pub Med. The results of 10 systematic reviews or meta-analyses and 18 primary studies of the in vitro research were recorded, summarized, and graphed.
Results: The review proved water washing combined with either APA and a primer or a cement with the phosphate-monomer 10-MDP as the reference protocol. Silica-coating resulted in an increase in the mean SBS from 8.45 MPa to 15.00 MPa without aging and from 6.41 MPa to 11.97 MPa after thermo cycling. While etching was found to generally underperform APA, it yielded better results with highly concentrated or heated acid systems. Laser pretreatment appears to favor bonding, with a pooled mean difference of 3.08 MPa, although Er: YAG Laser failed to deliver comparable results. Cold plasma pre-treatment resulted in an increase of the initial micro-shear bond strength from 21.6 MPa to 38.3 MPa . Saliva contamination was found to decrease the bond strength by as much as 38% in primer less conditions and re-abrasion was the most successful decontamination procedure.
Conclusion: The protocol of use of applying APA and 10-MDP appears as the best protocol, with the tribochemical silica coating as a good alternative. Conversely, laser, plasma and acid etching require further standardization and long-term data before adopting it in clinical practice